Burnout Cycles
Suggested Burnout Cycles

2-1/2” x 2-1/2”
(63 x 63mm)
|

3-1/2” x 4”
(89mm x 100mm)
|

4” x 8”
(100 x 200 mm)
|
1 hour - 300°F/149°C
1 hour - 700°F/371°C
2 hour - 1350°F/732°C
1 hour - Casting Temp. |
2 hour - 300°F/149°C
2 hour - 700°F/371°C
3 hour - 1350°F/732°C
1 hour - Casting Temp. |
2 hour - 300°F/149°C
2 hour - 700°F/371°C
3 hour - 1350°F/732°C
1 hour - Casting Temp. |
Casting
Temperatures
Ladies rings,
lacy or intricate designs,
900° - 1000°F (482° - 538°C).
Gents rings,
heavier designs,
700° - 900°F (371° - 482°C).
During the last 1 to 2 hours of burnout, the temperature
must be adjusted so that the flasks are at correct temperature
for casting.
|